Couldn't make .75 at 80ms work after switching batteries --needed to lower to 50ms as too much residual heat from increased | |
voltage off of a fresh battery. However, 40ms was insufficient heat to melt the wax, so the limiting factor comes down to the cooling. | |
Blowing on the device produced no noticeable difference. After a bit of reading, it seems that a thermoelectric cooler based on the peltier | |
effect is the likely solution. |